copper 200-220 france

Common raw materials

Forging display

CNC processing

- C18200 Alloy

Specific Gravity. 8.89. Electrical Conductivity % IACS at 68°F. 80 (1) Thermal Conductivity Btu/ sq ft/ ft hr/ °F at 68°F. 187 (2) Coefficient of Thermal Expansion 68-212 10 to -6

contact
Density lb/cu in. at 68°F: 0.321